Sample VT400 °C reveals a far more uniform particle size distribution and pores with an average grain measurement of about twelve nm (according to ImageJ application Investigation). On the flip side, changing deposition temperature to 700 °C bigger and denser particles with an average grain dimension of 460 nm was attained. Sample VT400 On th